Buy-side packaging specs
ECT vs Mullen: specifying corrugated boxes without overpaying
ECT (Edge Crush Test) measures how much edgewise compression the board takes, which predicts how well a box stacks. Mullen (burst test) measures how much pressure punctures the board, which tracks rough handling and liner weight. For boxes stacked on pallets, ECT is usually the right spec and often uses less fiber for the same stacking strength.
Published · Last updated
What does each test measure?
| ECT (Edge Crush Test) | Mullen (burst test) | |
|---|---|---|
| Measures | Force to crush a board sample on its edge, in pounds per inch | Pressure to burst through the board, in pounds per square inch |
| Predicts | Stacking (top-to-bottom compression) strength | Resistance to punctures and rough handling |
| Driven mostly by | The fluted medium and the overall board structure | The weight of the liners |
| Common single-wall ratings | 32 ECT, 44 ECT | 200#, 275# |
Where is the rating printed?
On the box maker's certificate, usually a round stamp on a bottom flap. It names the test used (edge crush or bursting test), the rating, and the size and gross weight limits the box is certified for. If a quoted box will carry a certificate, ask which one.
Are 32 ECT and 200# the same box?
No. Carrier rules have long allowed either test and pair them in the same row (32 ECT alongside 200# for single wall, 44 ECT alongside 275#), which is why they're often treated as equivalent. They measure different properties. A 200# box usually has heavier liners; a 32 ECT box can reach its rating with lighter liners and a stronger medium.
Which one should you specify?
- Boxes stacked on pallets in a warehouse: specify ECT. Stacking is how these boxes fail.
- Heavy, dense or sharp contents handled individually (parcel, rough handling): Mullen, or a higher ECT with a puncture test, may fit better.
- Humid storage or long dwell: stacking strength drops with moisture; ask suppliers about moisture-resistant board rather than just a higher number.
Can you estimate stacking strength from ECT?
Roughly. The McKee formula, widely used by box makers, estimates box compression strength from the board's ECT, its caliper (thickness) and the box perimeter:
box compression (lb) ≈ 5.87 × ECT × √(caliper in inches × perimeter in inches)
It's an estimate for regular slotted boxes in standard conditions. Real stacks lose strength to humidity, time, overhang off the pallet edge and handholes. Use it to ask better questions, not to sign off a spec.
How does this help you pay less?
Switching a stacked-load box from a Mullen spec to an equivalent-performing ECT spec is one of the common ways buyers reduce board cost, because it lets the box maker use less liner fiber. Ask suppliers to quote your current spec and an ECT alternative side by side, flag the alternative as a deviation, and test before switching.
See the corrugated boxes page for the full spec sheet, or start an RFQ.